Method for preparing Li

4x5-x1224x5-x12A method for preparing a LiNbTiO/C nanocomposite as anode material for lithium-ion batteries is disclosed, which includes the following steps: (a) obtaining a mixture of a lithium salt, niobium pentaoxide, titanium dioxide (TiO), and a carbon source in a selected stoichiometric ratio;...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: Hefei Guoxuan High-Tech Power Energy Co., Ltd
Format: Patent
Sprache:eng
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:4x5-x1224x5-x12A method for preparing a LiNbTiO/C nanocomposite as anode material for lithium-ion batteries is disclosed, which includes the following steps: (a) obtaining a mixture of a lithium salt, niobium pentaoxide, titanium dioxide (TiO), and a carbon source in a selected stoichiometric ratio; (b) mixing the mixture in a dispersant to produce a slurry; (c) drying the slurry to produce a dried mixture; (d) treating the dried mixture under a protective atmosphere, according to a heating program to produce the LiNbTiO/C nanocomposite, wherein the heating program comprises: calcining the dried mixture at 600° C. for 2-6 hours, heating it at a rate of 2-20° C. per minute to 950-980° C., cooling it by natural cooling to 800-850° C., maintaining the temperature at 800-850° C. for 16 hours, and cooling it by natural cooling to room temperature.