Aluminum engine cylinder liner and method
A method has been found for centrifugal casting engine cylinders. A mold is charged with molten aluminum alloy and particulate silicon monoxide having an average size of 0.01 mm to 0.04 mm. The mold is rotated at a velocity and period of time to distribute the particulate silicon monoxide on an inne...
Gespeichert in:
Hauptverfasser: | , |
---|---|
Format: | Patent |
Sprache: | eng |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A method has been found for centrifugal casting engine cylinders. A mold is charged with molten aluminum alloy and particulate silicon monoxide having an average size of 0.01 mm to 0.04 mm. The mold is rotated at a velocity and period of time to distribute the particulate silicon monoxide on an inner cylinder surface. The mold is allowed to cool until the aluminum alloy solidifies. A casting is demolded characterized in a uniform inner cylinder surface of the particulate silicon monoxide in an amount of 25 volume % and thickness 1 to 5 millimeters. The engine cylinders are distinguished in resistance to wear. Cylinder liners show no appreciable wear for over 100,000 miles of use. |
---|