Porous 4 group metal oxide and method for preparation thereof
(2-x)2x 2This invention relates to a 4 group metal oxide and to a method for preparation thereof and the 4 group metal oxide prepared by adding a particle growth inhibiter to a hydrosol a hydrogel or a dried product of a hydrous 4 group metal oxide represented by MO(OH)(wherein M denotes a 4 group m...
Gespeichert in:
Hauptverfasser: | , , , , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | (2-x)2x 2This invention relates to a 4 group metal oxide and to a method for preparation thereof and the 4 group metal oxide prepared by adding a particle growth inhibiter to a hydrosol a hydrogel or a dried product of a hydrous 4 group metal oxide represented by MO(OH)(wherein M denotes a 4 group metal and x is a number greater than 0.1 or x>0.1) followed by drying and calcining has a specific surface area of 80 m/g or more, a pore volume of 0.2 ml/g or more and a pore sharpness degree of 50% or more and excellent heat stability and is useful for a catalyst or a catalyst carrier in which a catalyst metal is dispersed to a high degree. This invention further relates to a porous 4 group metal oxide and to a method for preparation thereof and the 4 group metal oxide prepared by application of a pH swing operation is characterized by a large specific surface area, excellent heat stability, high dispersion of a catalyst metal and a controlled and sharp pore distribution and is useful for a catalyst or a catalyst carrier of excellent reaction selectivity. |
---|