Voice coil bobbin, manufacturing method thereof and speaker device
A voice coil bobbin is formed by skinpass rolling of pure titanium. A manufacturing method of a voice coil bobbin includes a process which manufactures a rolled pure titanium material, a process which executes skinpass rolling of the rolled material, and a process which forms the rolled material aft...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Patent |
Sprache: | eng |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | A voice coil bobbin is formed by skinpass rolling of pure titanium. A manufacturing method of a voice coil bobbin includes a process which manufactures a rolled pure titanium material, a process which executes skinpass rolling of the rolled material, and a process which forms the rolled material after the skinpass rolling to manufacture the voice coil bobbin. For example, the rolled pure titanium material is manufactured by a standard manufacturing process of a normal rolled material defined by JISH4600, and the cold rolling for the purpose of the strengthening is executed. The cold rolling is executed under a condition of a rolling ratio equal to or larger than 60%. Thereby, it becomes possible to obtain double hardness of JIS No. 1-kind titanium material (TR270C) and tensile strength larger than double of the JIS No. 1-kind titanium material (TR270C) and close to 6-4 titanium. By applying this thin voice coil bobbin with the high strength, the speaker device applicable for the high power input can be obtained. |
---|