Conversion of CO to CO2
Gold oxide is precipitated together with iron oxide from a solution containing a gold source and an iron source; the gel formed thereby is washed, dried, ground to a size range of 0.85 mm to 4.25 mm, calcined and activated by passing a hydrogen and oxygen containing gas through it; then used as a ca...
Gespeichert in:
1. Verfasser: | |
---|---|
Format: | Patent |
Sprache: | eng |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Gold oxide is precipitated together with iron oxide from a solution containing a gold source and an iron source; the gel formed thereby is washed, dried, ground to a size range of 0.85 mm to 4.25 mm, calcined and activated by passing a hydrogen and oxygen containing gas through it; then used as a catalyst for oxidizing CO to CO
2
in the presence of a large excess of hydrogen. |
---|