Propylene-based polymer and film made of the same

A propylene-based polymer having a melt flow rate of 0.1 to 20 g/10 min. and a melting point Tm (° C.) measured by using a differential scanning calorimeter (DSC) of 147 to 159° C., in which the half width HW (° C.) of the melting peak measured by using a differential scanning calorimeter (DSC) and...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Tsuji, Mitsuji, Yada, Kenichiro, Yunoki, Syunji
Format: Patent
Sprache:eng
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A propylene-based polymer having a melt flow rate of 0.1 to 20 g/10 min. and a melting point Tm (° C.) measured by using a differential scanning calorimeter (DSC) of 147 to 159° C., in which the half width HW (° C.) of the melting peak measured by using a differential scanning calorimeter (DSC) and the melting point Tm (° C.) satisfy the relation: HW (188−Tm)/5.