Stepwise pyrolysis of mixed plastics and paper for separation of oxygenated and hydrocarbon condensates

[Display omitted] •Stepwise pyrolysis at 350 and 500 °C can separate products into two fractions.•First step liquid product was acidic and had high amounts of oxygenated compounds.•Products from the second step had high hydrocarbon contents and low acidity.•Interaction between cellulose and plastics...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Applied energy 2018-11, Vol.229, p.314-325
Hauptverfasser: Sophonrat, Nanta, Sandström, Linda, Zaini, Ilman Nuran, Yang, Weihong
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:[Display omitted] •Stepwise pyrolysis at 350 and 500 °C can separate products into two fractions.•First step liquid product was acidic and had high amounts of oxygenated compounds.•Products from the second step had high hydrocarbon contents and low acidity.•Interaction between cellulose and plastics during stepwise pyrolysis was observed.•Test on real wastes and discussion of scaling-up possibilities were presented. Mixed plastics and papers are two of the main fractions in municipal solid waste which is a critical environmental issue today. Recovering energy and chemicals from this waste stream by pyrolysis is one of the favorable options to achieve a circular economy. While pyrolysis products from plastics are mainly hydrocarbons, pyrolysis products from paper/biomass are highly oxygenated. The different nature of the two pyrolysis products results in different treatments and applications as well as economic values. Therefore, separation of these two products by multi-step pyrolysis based on their different decomposition temperatures could be beneficial for downstream processes to recover materials, chemicals and/or energy. In this work, stepwise pyrolysis of mixed plastics and paper waste was performed in a batch type fixed bed reactor using two different pyrolysis temperatures. Neat plastic materials (polystyrene, polyethylene) and cellulose mixtures were used as starting materials. Then, the same conditions were applied to a mixed plastics and paper residue stream derived from paper recycling process. The condensable products were analyzed by GC/MS. It was found that pyrolysis temperatures during the first and second step of 350 and 500 °C resulted in a better separation of the oxygenated and hydrocarbon condensates than when a lower pyrolysis temperature (300 °C) was used in the first step. The products from the first step were derived from cellulose with some heavy fraction of styrene oligomers, while the products from the second step were mainly hydrocarbons derived from polystyrene and polyethylene. This thus shows that stepwise pyrolysis can separate the products from these materials, although with some degree of overlapping products. Indications of interaction between PS and cellulose during stepwise pyrolysis were observed including an increase in char yield, a decrease in liquid yield from the first temperature step and changes in liquid composition, compared to stepwise pyrolysis of the two materials separately. A longer vapor residence time
ISSN:0306-2619
1872-9118
1872-9118