Influence of Sintering Parameters on the Mechanical Performance of PM Steels Pre-Alloyed with Chromium

Powder grades pre-alloyed with 1.5-3 wt% chromium are suitable for PM steel components in high performance applications. These materials can be successfully sintered at the conventional temperature 1120 °C, although well-monitored sintering atmospheres with low oxygen partial pressures (

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Materials science forum 2007-01, Vol.534-536, p.545-548
Hauptverfasser: Lindqvist, Björn, Bergman, Ola, Bengtsson, Sven
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Powder grades pre-alloyed with 1.5-3 wt% chromium are suitable for PM steel components in high performance applications. These materials can be successfully sintered at the conventional temperature 1120 °C, although well-monitored sintering atmospheres with low oxygen partial pressures (