Microwave pyrolysis of multilayer plastic waste (LDPE) using zeolite catalyst
To overcome the problem of garbage, especially plastic waste, environmental experts and scholars from various disciplines have conducted various studies and actions. One way to degrade the multilayer packaging plastic waste LDPE (Low Density Poliethylene) with microwave pyrolysis process by using na...
Gespeichert in:
Hauptverfasser: | , , , |
---|---|
Format: | Tagungsbericht |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | To overcome the problem of garbage, especially plastic waste, environmental experts and scholars from various disciplines have conducted various studies and actions. One way to degrade the multilayer packaging plastic waste LDPE (Low Density Poliethylene) with microwave pyrolysis process by using natural zeolite catalysts. The purpose of this experiment was to determine the effect of temperature and time of microwave pyrolysis process by using natural zeolite catalyst to degrade the plastic waste LDPE and compare them. Pyrolysis process was done by using a closed glass reactor with a capacity of 500 ml, operated at a pressure of 1 atm and flowed nitrogen 0.5 1 / min. Plastic waste was LDPE, and natural zeolite was used as its catalyst. Sample was heated at temperature 300, 400, 500 or 550 °C and was kept during time variables of 45, 60, 75 and 90 minutes. Liquid product was analyzed by Gas Chromatography-Mass Spectrometry (GC-MS), raw material was analyzed by Fourier Transform Infrared (FTIR), and solid product was analyzed by X-Ray Fluorescene (XRF). From the experimental resulted in the best yield products of pyrolisis using natural zeolite at 550 °C and 90 minutes was 2.88 % of solid yield, 28.12 % of liquid yield and the highest hydrocarbon concentration of 19.02 %. |
---|---|
ISSN: | 0094-243X 1551-7616 |
DOI: | 10.1063/1.4982331 |