Excellent microwave absorption properties by tuned electromagnetic parameters in polyaniline-coated Ba0.9La0.1Fe11.9Ni0.1O19/reduced graphene oxide nanocomposites

Ba 0.9 La 0.1 Fe 11.9 Ni 0.1 O 19 nanoparticles were prepared by a co-precipitation method, and Ba 0.9 La 0.1 Fe 11.9 Ni 0.1 O 19 /reduced graphene oxide/polyaniline ternary nanocomposites (BF/RGO/PANI) were prepared by in situ polymerization. Microwave reflection loss, and the permittivity and perm...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: Luo, Juhua, Zuo, Yue, Shen, Pan, Yan, Zhu, Zhang, Kang
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Ba 0.9 La 0.1 Fe 11.9 Ni 0.1 O 19 nanoparticles were prepared by a co-precipitation method, and Ba 0.9 La 0.1 Fe 11.9 Ni 0.1 O 19 /reduced graphene oxide/polyaniline ternary nanocomposites (BF/RGO/PANI) were prepared by in situ polymerization. Microwave reflection loss, and the permittivity and permeability of BF/RGO/PANI nanocomposites were investigated in the frequency range 2-18 GHz. The prepared samples possessed excellent electromagnetic wave-absorbing performances, and the optimal impedance matching of BF/RGO/PANI nanocomposites was found. The minimum reflection loss reached −49.1 dB near the frequency of 14.08 GHz with a thickness of 1.9 mm and its absorption bandwidth with a reflection loss below −10 dB ranged from 12.4-16.72 GHz with a bandwidth of 4.32 GHz. Our study illustrates that the as-prepared BF/RGO/PANI nanocomposites are promising candidates for use in electromagnetic wave-absorbing materials. The obvious enhancement of microwave absorption performance of Ba 0.9 La 0.1 Fe 11.9 Ni 0.1 O 19 /reduced graphene oxide/polyaniline ternary nanocomposites in 2-18 GHz was observed. The minimum reflection loss can reach −49.1 dB with thickness of 1.9 mm.
ISSN:2046-2069
DOI:10.1039/c7ra06800j