Influence of Silica Modulus and Curing Temperature on the Strength of Alkali-Activated Volcanic Ash and Limestone Powder Mortar

This present study evaluates the effect of silica modulus (Ms) and curing temperature on strengths and the microstructures of binary blended alkali-activated volcanic ash and limestone powder mortar. Mortar samples were prepared using mass ratio of combined Na2SiO3(aq)/10 M NaOH(aq) of 0.5 to 1.5 at...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Materials 2021-09, Vol.14 (18), p.5204
Hauptverfasser: Adewumi, Adeshina Adewale, Mohd Ariffin, Mohd Azreen, Maslehuddin, Mohammed, Yusuf, Moruf Olalekan, Ismail, Mohammad, Al-Sodani, Khaled A. Alawi
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:This present study evaluates the effect of silica modulus (Ms) and curing temperature on strengths and the microstructures of binary blended alkali-activated volcanic ash and limestone powder mortar. Mortar samples were prepared using mass ratio of combined Na2SiO3(aq)/10 M NaOH(aq) of 0.5 to 1.5 at an interval of 0.25, corresponding to Ms of 0.52, 0.72, 0.89, 1.05 and 1.18, respectively, and sole 10 M NaOH(aq). Samples were then subjected to ambient room temperature, and the oven-cured temperature was maintained from 45 to 90 °C at an interval of 15 °C for 24 h. The maximum achievable 28-day strength was 27 MPa at Ms value of 0.89 cured at 75 °C. Samples synthesised with the sole 10 M NaOH(aq) activator resulted in a binder with a low 28-day compressive strength (15 MPa) compared to combined usage of Na2SiO3(aq)/10 M NaOH(aq) activators. Results further revealed that curing at low temperatures (25 °C to 45 °C) does not favour strength development, whereas higher curing temperature positively enhanced strength development. More than 70% of the 28-day compressive strength could be achieved within 12 h of curing with the usage of combined Na2SiO3(aq)/10 M NaOH(aq). XRD, FTIR and SEM + EDX characterisations revealed that activation with combined Na2SiO3(aq)/10 M NaOH(aq) leads to the formation of anorthite (CaAl2Si2O8), gehlenite (CaO.Al2O3.SiO2) and albite (NaAlSi3O8) that improve the amorphosity, homogeneity and microstructural density of the binder compared to that of samples synthesised with sole 10 M NaOH(aq).