The Corrosion Probability and Flexural Strength of an RC Beam under Chloride Ingress Considering the Randomness of Temperature and Humidity
The load capacity of reinforced concrete structure will decrease by chloride ingress in coastal region. In this paper, the corrosion probability and flexural strength of a typical reinforced concrete beam design under the influence of temperature and humidity was obtained by the Monte Carlo method....
Gespeichert in:
Veröffentlicht in: | Materials 2020-05, Vol.13 (10), p.2260 |
---|---|
Hauptverfasser: | , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The load capacity of reinforced concrete structure will decrease by chloride ingress in coastal region. In this paper, the corrosion probability and flexural strength of a typical reinforced concrete beam design under the influence of temperature and humidity was obtained by the Monte Carlo method. The relationship between flexural strength, temperature, relative humidity, and geometric parameters was established. The annual average temperature and relative humidity were treated as random variables together with the geometric size and concrete compressive strength. The corrosion probability and flexural strength in a wave splashing zone, coastal atmospheric zone, and offshore atmospheric zone were calculated. The results show that the corrosion probabilities of the three regions are obviously different. When the standard deviation of temperature is less than 1.5 °C, the temperature can be treated as a constant in the calculation of the concrete cracking probability in the wave splashing zone. A binary logistic regression formula was given to predict whether the randomness of temperature and humidity should be considered in the offshore atmospheric zone. When the standard deviation of the temperature is less than 1 °C, the temperature randomness has no significant effect on the flexural strength of beams in the wave splashing zone. The flexural strength distribution conforms to the normal distribution in the early stage of service and the Weibull distribution after concrete cracking. |
---|---|
ISSN: | 1996-1944 1996-1944 |
DOI: | 10.3390/ma13102260 |