Preparation and Properties of Rubber Blends for High-Damping-Isolation Bearings
To improve the energy dissipation capacity of rubber isolation bearings, it is important to find a new rubber material with good applicability and high damping properties. Two types of blends were prepared using nitrile rubber (NBR), brominated butyl rubber (BIIR) and ethylene-vinyl acetate copolyme...
Gespeichert in:
Veröffentlicht in: | Polymers 2019-08, Vol.11 (8), p.1374 |
---|---|
Hauptverfasser: | , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | To improve the energy dissipation capacity of rubber isolation bearings, it is important to find a new rubber material with good applicability and high damping properties. Two types of blends were prepared using nitrile rubber (NBR), brominated butyl rubber (BIIR) and ethylene-vinyl acetate copolymer (EVA): NBR/BIIR and NBR/BIIR/EVA. The vulcanization, mechanical and damping properties of the blends were analyzed. The results show that both blends exhibit excellent vulcanization plateaus and mechanical properties. For NBR/BIIR, as the BIIR content increases, the complementary effects of NBR and BIIR afforded by blending are enhanced. Two damping peaks appeared in the tanδ-T curve and shifted toward lower and higher temperatures, respectively, which clearly widened the effective damping temperature range. However, the damping value in the valley of the tanδ-T curve was as low as 0.39. For NBR/BIIR/EVA, the addition of EVA greatly increased damping in the valley of the tanδ-T curve to approximately 0.54. EVA was observed to be the optimal polymer for improving the compatibility of the NBR/BIIR blend. Moreover, hot air thermal aging tests showed that both blends demonstrated good stability. |
---|---|
ISSN: | 2073-4360 2073-4360 |
DOI: | 10.3390/polym11081374 |