Comparative evaluation of shear bond strength of three flowable compomers on enamel of primary teeth: An in-vitro study

The aim of the present study was to determine Shear bond strength (SBS) of different flowable compomers on the enamel surface of primary teeth. The null hypothesis to be tested was that none of the flowable compomer would differ significantly from the other two with respect to SBS. As a result, the...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of clinical and experimental dentistry 2016-07, Vol.8 (3), p.e322-e326
Hauptverfasser: Gungor, OE, Erdogan, Y, Yalçın-Gungor, A, Alkis, H
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The aim of the present study was to determine Shear bond strength (SBS) of different flowable compomers on the enamel surface of primary teeth. The null hypothesis to be tested was that none of the flowable compomer would differ significantly from the other two with respect to SBS. As a result, the tested materials that have the easiest application on child patient is preferred. Sixty newly extracted non carious primary molars were selected. The buccal surface was cleaned and polished to obtain a flat enamel surface. The specimens were randomly divided into three groups of 20 teeth each, based on the flowable compomers applied, as follows: group I: Dyract Flow® (Dentsply, Konstanz, Germany); group II: Twinky Star Flow® (Voco, Cuxhaven, Germany); and group III: R&D Series Nova Compomer Flow® (Imicryl, Konya, Turkey). SBS in group II (6.78± 0.45 MPa) were significantly lower than groups I and III (8.30 ± 0.29 and 8.43 ± 0.66 MPa, respectively) (P
ISSN:1989-5488
1989-5488
DOI:10.4317/jced.52785