Thin Hard Crest on the Edge of Ceramic Acetabular Liners Accelerates Wear in Edge Loading

Abstract Ceramic acetabular liners may exhibit a small, sharp crest—an artifact of discontinuous machining steps—at the junction between the concave spherical surface and the interior edge. On 3 ceramic liners, this crest was found to form a 9° to 11° deviation from tangency. Edge loading wear tests...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:The Journal of arthroplasty 2012-01, Vol.27 (1), p.150-152
Hauptverfasser: Sanders, Anthony P., MS, Dudhiya, Parth J., BTech, Brannon, Rebecca M., PhD
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Abstract Ceramic acetabular liners may exhibit a small, sharp crest—an artifact of discontinuous machining steps—at the junction between the concave spherical surface and the interior edge. On 3 ceramic liners, this crest was found to form a 9° to 11° deviation from tangency. Edge loading wear tests were conducted directly on this crest and on a smoother region of the edge. The crest elicited 2 to 15 times greater volumetric wear on the femoral head. The propensity of the crest to rapidly (
ISSN:0883-5403
1532-8406
DOI:10.1016/j.arth.2011.08.012