Do Different Pretreatments of Dentine Surface Affect the Bond Strength with a Self-adhesive Resin Cement?
To evaluate the microtensile bond strength of dentine/self-adhesive resin cement interface after several treatments on a dentine surface. Twenty-eight human molars were selected and divided into four groups: no treatment (control (C)); 2% chlorhexidine digluconate (CHX); 25% polyacrylic acid (PA); a...
Gespeichert in:
Veröffentlicht in: | Oral health & preventive dentistry 2020-04, Vol.18 (2), p.145 |
---|---|
Hauptverfasser: | , , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | To evaluate the microtensile bond strength of dentine/self-adhesive resin cement interface after several treatments on a dentine surface.
Twenty-eight human molars were selected and divided into four groups: no treatment (control (C)); 2% chlorhexidine digluconate (CHX); 25% polyacrylic acid (PA); and 23 ppm dispersive solution of silver nanoparticle (SN). Prepolymerised TPH resin composite (Dentsply) blocks were luted on the dentine surface using RelyX U200 self-adhesive resin cement (3M ESPE). Microtensile bond strength was measured (MPa) in a universal testing machine 24 h and 6 months after the bonding process. The fractured specimens were examined in an optical microscope and classified according to the fracture pattern. A representative sample of each group was observed by scanning electronic microscope. Data were submitted to analysis of variance (ANOVA) and Tukey's test to compare the mean among the groups (p |
---|---|