Effect of K-wire Reuse and Drill Mode on Heat Generation in Bone

Background We examined the effect of Kirschner wire (K-wire) reuse and use of oscillating mode on heat generation within cortical bone. Methods Two trocar-tipped K-wires were drilled through the diaphysis of each of 30 human metacarpals and phalanges: one K-wire was inserted in rotary mode and anoth...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Hand (New York, N.Y.) N.Y.), 2023-03, Vol.18 (2), p.314-319
Hauptverfasser: Muriuki, Muturi G., Reddy, Arun K., Tauchen, Alex, Havey, Robert M., Patwardhan, Avinash G., Bindra, Randy R.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Background We examined the effect of Kirschner wire (K-wire) reuse and use of oscillating mode on heat generation within cortical bone. Methods Two trocar-tipped K-wires were drilled through the diaphysis of each of 30 human metacarpals and phalanges: one K-wire was inserted in rotary mode and another in oscillating mode. Each wire was reused once. Thermocouples placed within the dorsal and volar bone adjacent to the K-wire drill path measured temperatures throughout each test. Results Peak cortex temperatures were 25°C to 164°C. Rotary drilling achieves peak temperatures quicker (31 ± 78 seconds vs 44 ± 78 seconds, P = .19) than oscillating drilling, but insertion time is also less, resulting in lower overall heat exposure. This effect is also seen when the K-wire is reused (34 ± 70 seconds vs 41 ± 85 seconds, P = .4). The length of time that cortical bone was exposed to critical temperatures (47°C or more) was significantly higher when a wire was reused (36 ± 72 seconds vs 43 ± 82 seconds, P = .008). Peak temperatures greater than 70°C (a temperature associated with instantaneous cell death) were observed on many occasions. Conclusions Overall heat exposure may be higher if a K-wire is reused or inserted in oscillating mode. In the absence of external cooling, K-wire insertion into cortical bone can easily expose bone to temperatures that exceed 70°C and may increase the risk of osteonecrosis.
ISSN:1558-9447
1558-9455
DOI:10.1177/15589447211003172