Phase Structure, Bond Features, and Microwave Dielectric Characteristics of Ruddlesden-Popper Type Sr 2 TiO 4 Ceramics
This work studied the phase constitution, bond characteristics, and microwave dielectric performances of Sr TiO ceramics. Based on XRD and Rietveld refinement analysis, pure tetragonal Ruddlesden-Popper type Sr TiO ceramic is synthesized at 1425~1525 °C. Meanwhile, the microstructure is dense and wi...
Gespeichert in:
Veröffentlicht in: | Materials 2023-07, Vol.16 (14) |
---|---|
Hauptverfasser: | , , , , , , , |
Format: | Artikel |
Sprache: | eng |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | This work studied the phase constitution, bond characteristics, and microwave dielectric performances of Sr
TiO
ceramics. Based on XRD and Rietveld refinement analysis, pure tetragonal Ruddlesden-Popper type Sr
TiO
ceramic is synthesized at 1425~1525 °C. Meanwhile, the microstructure is dense and without porosity, indicating its high sinterability and densification. Great microwave dielectric performances can be obtained, namely an
value of 39.41, and a
value of 93,120 GHz, when sintered at 1475 °C. Under ideal sintering conditions, the extrinsic factors are minimized and can be ignored. Thus, the intrinsic factors are considered crucial in determining microwave dielectric performances. Based on the P-V-L complex chemical bond theory calculation, the largest bond ionicity, and proportions to the bond susceptibility from Sr-O bonds suggest that Sr-O bonds mainly determine the dielectric polarizability. However, the Ti-O bonds show lattice energy about three times larger than Sr-O bonds, emphasizing that the structural stability of Sr
TiO
ceramics is dominated by Ti-O bonds, and the Ti-O bonds are vital in determining the intrinsic dielectric loss. The thermal expansion coefficient value of the Sr
TiO
structure is also mainly decided by Ti-O bonds. |
---|---|
ISSN: | 1996-1944 1996-1944 |