Extruded materials for thermoelectric coolers

We have optimized the compositions of p -type thermoelectric materials based on solid solutions between bismuth and antimony tellurides with high thermoelectric figures of merit in different temperature ranges between 100 and 300 K. The materials have been prepared by extrusion and have been charact...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Inorganic materials 2008-07, Vol.44 (7), p.687-691
Hauptverfasser: Ivanova, L. D., Petrova, L. I., Granatkina, Yu. V., Zemskov, V. S., Sokolov, O. B., Skipidarov, S. Ya, Duvankov, N. I.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:We have optimized the compositions of p -type thermoelectric materials based on solid solutions between bismuth and antimony tellurides with high thermoelectric figures of merit in different temperature ranges between 100 and 300 K. The materials have been prepared by extrusion and have been characterized by microstructural analysis. Their thermoelectric properties have been studied in the range 100–400 K.
ISSN:0020-1685
1608-3172
DOI:10.1134/S0020168508070030