Anelastic deformation measurements in structural engineering alloys

Nonelastic strains in the form of room-temperature primary creep and anelasticity occur at 70 percent of the yield strength for 4340 steel, 15-5 PH, 304 stainless steel, Ti6Al4V, and NILO 365. The amount of creep (the irrecoverable strain) diminishes with loading cycle due to work hardening. The ane...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of materials engineering and performance 2000-08, Vol.9 (4), p.463-466
1. Verfasser: COTTON, J. D
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Nonelastic strains in the form of room-temperature primary creep and anelasticity occur at 70 percent of the yield strength for 4340 steel, 15-5 PH, 304 stainless steel, Ti6Al4V, and NILO 365. The amount of creep (the irrecoverable strain) diminishes with loading cycle due to work hardening. The anelastic strains are relatively constant for each loading cycle, about 25 micro-epsilon for ferrous alloys and 4 micro-epsilon for Ti6Al4V. The anelastic beahvior for NILO 365 was anomalous, presumably due to magnetostriction effects. (CSA)