Solar evaporation enhancement using floating light-absorbing magnetic particles

We have demonstrated a new strategy for enhancing solar evaporation by using floating light-absorbing materials. Floating Fe3O4/C magnetic particles with an average size of 500 nm were synthesized by carbonization of poly(furfuryl alcohol) (PFA) incorporated with Fe3O4 nanoparticles. The Fe3O4/C par...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Energy & environmental science 2011-01, Vol.4 (10), p.4074-4078
Hauptverfasser: Zeng, Yao, Yao, Jianfeng, Horri, Bahman Amini, Wang, Kun, Wu, Yuzhou, Li, Dan, Wang, Huanting
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:We have demonstrated a new strategy for enhancing solar evaporation by using floating light-absorbing materials. Floating Fe3O4/C magnetic particles with an average size of 500 nm were synthesized by carbonization of poly(furfuryl alcohol) (PFA) incorporated with Fe3O4 nanoparticles. The Fe3O4/C particles had a BET surface area of 429 m2 g-1, and a density of 1.44 g cm-3. Because of their hydrophobicity and a bulk packing density of 0.53 g cm-3, Fe3O4/C particles were floatable on water. Our results indicated that these Fe3O4/C particles enhanced the water evaporation rate by as much as a factor of 2.3 in the solar evaporation of 3.5% salt water. In addition, Fe3O4/C particles were easily recycled using a magnet, and stable after being recycled three times. Our work provides a low-cost and highly effective way for accelerating solar evaporation for industrial applications such as solar desalination, salt production, brine management and wastewater treatment.
ISSN:1754-5692
1754-5706