Hydroxyapatite whisker-reinforced polyetherketoneketone bone ingrowth scaffolds
Hydroxyapatite (HA) whisker-reinforced polyetherketoneketone (PEKK) bone ingrowth scaffolds were prepared and characterized. High levels of porosity (75–90%) and HA whisker reinforcement (0–40 vol.%) were attained using a powder processing approach to mix the HA whiskers, PEKK powder and a NaCl poro...
Gespeichert in:
Veröffentlicht in: | Acta biomaterialia 2010-03, Vol.6 (3), p.856-863 |
---|---|
Hauptverfasser: | , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Hydroxyapatite (HA) whisker-reinforced polyetherketoneketone (PEKK) bone ingrowth scaffolds were prepared and characterized. High levels of porosity (75–90%) and HA whisker reinforcement (0–40 vol.%) were attained using a powder processing approach to mix the HA whiskers, PEKK powder and a NaCl porogen, followed by compression molding at 350–375
°C and particle leaching to remove the porogen. The scaffold architecture and microstructure exhibited characteristics known to be favorable for osteointegration. Scaffold porosity was interconnected with a mean pore size in the range 200–300
μm as measured by micro-computed tomography. HA whiskers were embedded within and exposed on the surface of scaffold struts, producing a microscale surface topography, shown by von Kossa staining and scanning electron microscopy. Therefore, HA whisker-reinforced PEKK bone ingrowth scaffolds may be advantageous for orthopedic implant fixation, including interbody spinal fusion. |
---|---|