Effect of thermal annealing time on optical and structural properties of TeO sub(2 thin films)
TeO sub(2 thin films were deposited on quartz substrates by rf reactive sputtering technique from a te metal target. The obtained samples were annealed in an argon atmosphere at 450 degree C for different annealing times up to 90 min. X-ray diffraction studies revealed that the as-grown samples were...
Gespeichert in:
Veröffentlicht in: | Vacuum 2010-03, Vol.84 (7), p.935-939 |
---|---|
Hauptverfasser: | , , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | TeO sub(2 thin films were deposited on quartz substrates by rf reactive sputtering technique from a te metal target. The obtained samples were annealed in an argon atmosphere at 450 degree C for different annealing times up to 90 min. X-ray diffraction studies revealed that the as-grown samples were amorphous and there was no appreciable change in structure for a short annealing time. Thin films became polycrystalline with the tetragonal ( alpha -phase) structure of tellurium dioxide crystal with the increase of the thermal annealing time. The refractive index and optical energy gap of the films were calculated by modelling transmittance spectra. The optical energy gap decreased continuously from 3.83 eV to 3.71 eV with increasing thermal annealing time.) |
---|---|
ISSN: | 0042-207X |
DOI: | 10.1016/j.vacuum.2009.12.017 |