Combustion synthesis of Ni, Fe and Cu multi-component catalysts for hydrogen production from ethanol reforming

[Display omitted] ► Ni 1Fe 0.5Cu 1 is the most active composition. ► The activity–selectivity of Cu, Ni and Fe varied with T. ► Ni is selective for H 2 and CH 4, Cu for CH 3CHO and H 2, and Fe for H 2 and C 2H 6. Solution combustion synthesis was used to prepare multi-component catalysts containing...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Applied catalysis. A, General General, 2011-07, Vol.401 (1), p.20-28
Hauptverfasser: Kumar, A., Mukasyan, A.S., Wolf, E.E.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:[Display omitted] ► Ni 1Fe 0.5Cu 1 is the most active composition. ► The activity–selectivity of Cu, Ni and Fe varied with T. ► Ni is selective for H 2 and CH 4, Cu for CH 3CHO and H 2, and Fe for H 2 and C 2H 6. Solution combustion synthesis was used to prepare multi-component catalysts containing Ni, Fe, and Cu using a controlled volume combustion method. A series of catalysts containing the selected metals in different molar ratios were analyzed for their activity and hydrogen selectivity for ethanol decomposition and ethanol partial oxidative reforming reactions. The most active and selective catalyst was found to be Ni 1Fe 0.5Cu 1 yielding ∼80% conversion and ∼42% hydrogen selectivity at the relatively low temperature of ∼415 °C for the ethanol decomposition reaction. Decreasing the oxygen concentration in the feed increased the H 2 selectivity at lower temperature. In the absence of oxygen, i.e. during ethanol decomposition, hydrogen production starts at 120 °C and gives a selectivity of ∼40% at about 380 °C. Studies with monometallic catalysts show that Ni at lower temperature was the most active and selective for hydrogen and methane, Cu was selective for acetaldehyde and Fe was selective for CO 2 and ethane. Hydrogen selectivity was found to be highest for Fe at high temperature.
ISSN:0926-860X
1873-3875
DOI:10.1016/j.apcata.2011.04.038