Flash grain welding in yttria stabilized zirconia

Self-standing samples made of isostatically pressed powders of ZrO 2:8 mol% Y 2O 3 were submitted to AC signals of 60 and 1000 Hz. At temperatures of around 900 °C, a current density exceeding approximately 100 mA/cm 2 starts an avalanche process with a fast increasing current under constant voltage...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of the European Ceramic Society 2011-07, Vol.31 (8), p.1517-1521
Hauptverfasser: Muccillo, Reginaldo, Kleitz, Michel, Muccillo, Eliana N.S.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Self-standing samples made of isostatically pressed powders of ZrO 2:8 mol% Y 2O 3 were submitted to AC signals of 60 and 1000 Hz. At temperatures of around 900 °C, a current density exceeding approximately 100 mA/cm 2 starts an avalanche process with a fast increasing current under constant voltage. It lasts about 60 s and it is preceded by an induction period of the order of 30 s. After that, the material is sintered as confirmed by impedance diagrams. Relative densities of 94% could be obtained.
ISSN:0955-2219