Influence of alkali metal modification and reaction conditions on the catalytic activity and stability of Ni containing smectite-type material for steam reforming of acetic acid

A Ni incorporated mesoporous smectite-like material, SM(Ni), was modified by various alkali metals, such as, Li, Na, K, Rb or Cs, and tested for the steam reforming of acetic acid as a model compound of aqueous phase of bio-oil derived from biomass pyrolysis. Initial conversion of acetic acid and co...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:International journal of hydrogen energy 2011-05, Vol.36 (10), p.5904-5911
Hauptverfasser: Iwasa, Nobuhiro, Yamane, Toshiyuki, Arai, Masahiko
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:A Ni incorporated mesoporous smectite-like material, SM(Ni), was modified by various alkali metals, such as, Li, Na, K, Rb or Cs, and tested for the steam reforming of acetic acid as a model compound of aqueous phase of bio-oil derived from biomass pyrolysis. Initial conversion of acetic acid and concentration of H 2 produced are drastically enhanced by the modification with these alkali metals. 1.0 wt% K-modified SM(Ni) catalyst exhibits the highest activity among the modified SM(Ni) materials tested. Addition of K promotes the reduction of Ni species incorporated in the smectite, yielding more metallic Ni species than in the original SM(Ni) sample. Therefore, the K-modified SM(Ni) catalyst gives higher initial activity compared with the original smectite catalyst. However, these modified materials lose their activities due to carbon deposition on their surface during the course of reaction, similar to the original SM(Ni). The influence of reaction conditions, such as O 2 or H 2 addition, steam to carbon ratio (S/C) and reaction temperature, was also investigated. Higher and more stable activity was obtained with unmodified SM(Ni) catalyst at a high reaction temperature of 973 K and at an S/C ratio of 3.3.
ISSN:0360-3199