Retention of Freon in poly(n-butyl α-cyanoacrylate) sprayed films
It has been found that when n‐butyl α‐cyanoacrylate is sprayed on a blood surface from an aerosol containing Freon as the propellant, the polymeric cyanoacrylate film which forms contains 1.4% propellant under the spray conditions used. Studies of the rate of loss of propellant from the film indicat...
Gespeichert in:
Veröffentlicht in: | Journal of biomedical materials research 1969-06, Vol.3 (2), p.267-271 |
---|---|
Hauptverfasser: | , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | It has been found that when n‐butyl α‐cyanoacrylate is sprayed on a blood surface from an aerosol containing Freon as the propellant, the polymeric cyanoacrylate film which forms contains 1.4% propellant under the spray conditions used. Studies of the rate of loss of propellant from the film indicate that ⅓ of the Freon initially present in the film still remains after 90 min of exposure of the film to air. Possible implications of these results are discussed. |
---|---|
ISSN: | 0021-9304 1097-4636 |
DOI: | 10.1002/jbm.820030206 |