Retention of Freon in poly(n-butyl α-cyanoacrylate) sprayed films

It has been found that when n‐butyl α‐cyanoacrylate is sprayed on a blood surface from an aerosol containing Freon as the propellant, the polymeric cyanoacrylate film which forms contains 1.4% propellant under the spray conditions used. Studies of the rate of loss of propellant from the film indicat...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of biomedical materials research 1969-06, Vol.3 (2), p.267-271
Hauptverfasser: Leonard, Fred, Lusardi, Joseph J., Kulkarni, Ramchandra K., Wade, Clarence W. R.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:It has been found that when n‐butyl α‐cyanoacrylate is sprayed on a blood surface from an aerosol containing Freon as the propellant, the polymeric cyanoacrylate film which forms contains 1.4% propellant under the spray conditions used. Studies of the rate of loss of propellant from the film indicate that ⅓ of the Freon initially present in the film still remains after 90 min of exposure of the film to air. Possible implications of these results are discussed.
ISSN:0021-9304
1097-4636
DOI:10.1002/jbm.820030206