Industrial scale-up of pH-controlled liquid hot water pretreatment of corn fiber for fuel ethanol production

The pretreatment of cellulose in corn fiber by liquid hot water at 160 °C and a pH above 4.0 dissolved 50% of the fiber in 20 min. The pretreatment also enabled the subsequent complete enzymatic hydrolysis of the remaining polysaccharides to monosaccharides. The carbohydrates dissolved by the pretre...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Applied biochemistry and biotechnology 2005-05, Vol.125 (2), p.77-98
Hauptverfasser: Mosier, N.S, Hendrickson, R, Brewer, M, Ho, N, Sedlak, M, Dreshel, R, Welch, G, Dien, B.S, Aden, A, Ladisch, M.R
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The pretreatment of cellulose in corn fiber by liquid hot water at 160 °C and a pH above 4.0 dissolved 50% of the fiber in 20 min. The pretreatment also enabled the subsequent complete enzymatic hydrolysis of the remaining polysaccharides to monosaccharides. The carbohydrates dissolved by the pretreatment were 80% soluble oligosaccharides and 20% monosaccharides with 90% of theoretical based on the starting fiber. This cooperative effort and first successful trial opens the door for examining the robustness of the pretreatment system under extended run conditions as well as pretreatment of other cellulose-containing materials using water at controlled pH.
ISSN:0273-2289