This study aims to enhance the endurance of MoS2 coating by applying a thin layer of Au (a arrow right 480nm) on MoS2 surface. Experimental results show that the addition of Au film increases the endurance of MoS2/Au over equivalent coatings without Au. The friction coefficient rapidly decreases to...
Gespeichert in:
Veröffentlicht in: | Thin solid films 2010-10, Vol.518 (24), p.7532-7534 |
---|---|
Hauptverfasser: | , , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | This study aims to enhance the endurance of MoS2 coating by applying a thin layer of Au (a arrow right 480nm) on MoS2 surface. Experimental results show that the addition of Au film increases the endurance of MoS2/Au over equivalent coatings without Au. The friction coefficient rapidly decreases to a stable value (I14 a arrow right 40.045) after about 100cycles sliding. After more than 15,000cycles, the friction coefficient gradually increased to a second stable value (I14 a arrow right 40.15). An average endurance of over 50,000cycles was measured in this case. The Au or Au-MoS2 composite layer can effectively prevent oxygen or moisture reaction with MoS2 and hence significantly increases the wear life. |
---|---|
ISSN: | 0040-6090 1879-2731 |
DOI: | 10.1016/j.tsf.2010.05.040 |