Optimization of a Weld Overlay on a Plate Structure
An overlay weld repair procedure on a 1066.8X1066.8 mm2 square plate 25.4 mm thick was simulated to compute the 3D transient temperature, microstructure, strain, stress, and displacement of the overlay weld repair procedure. The application for the overlay was the repair of cavitation erosion damage...
Gespeichert in:
Veröffentlicht in: | Journal of pressure vessel technology 2010-02, Vol.132 (1), p.011402 (9 )-011402 (9 ) |
---|---|
Hauptverfasser: | , , , , |
Format: | Artikel |
Sprache: | eng |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | An overlay weld repair procedure on a 1066.8X1066.8 mm2 square plate 25.4 mm thick was simulated to compute the 3D transient temperature, microstructure, strain, stress, and displacement of the overlay weld repair procedure. The application for the overlay was the repair of cavitation erosion damage on a large Francis turbine used in a hydroelectric project. The overlay weld consisted of a 4X6 pattern of 100X100 mm2 squares. Each square was covered by 15 weld passes. Each weld pass was 100 mm long. The total length of weld in the six squares was 36 m. The welds in each square were oriented either front-to-back or left-to-right. The welding process was shielded metal arc. The analysis shows that alternating the welding direction in each square produces the least distortion. A delay time of 950 s between the end of one weld pass and the start of the next weld pass was imposed to meet the requirement of a maximum interpass temperature to 50 deg C. |
---|---|
ISSN: | 0094-9930 |
DOI: | 10.1115/1.4000511YouarenotloggedintotheASMEDigitalLibrary. |