Targetry of SrCO(3) on a copper substrate by sedimentation method for the cyclotron production no-carrier-added (86)Y

Strontium carbonate deposition on copper substrate was carried out by the sedimentation method in order to produce yttrium-86. Natural strontium carbonate thick layer was prepared with 480 mg SrCO(3), 220 mg ethyl cellulose, and 7.5 mL acetone. This optimum condition is a result of several repeated...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Applied radiation and isotopes 2009-11, Vol.67 (11), p.2029-2032
Hauptverfasser: Sadeghi, M, Zali, A, Aboudzadeh, M, Sarabadani, P, Aslani, G, Majdabadi, A
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Strontium carbonate deposition on copper substrate was carried out by the sedimentation method in order to produce yttrium-86. Natural strontium carbonate thick layer was prepared with 480 mg SrCO(3), 220 mg ethyl cellulose, and 7.5 mL acetone. This optimum condition is a result of several repeated experiments with different amount of ethyl cellulose and acetone. Target quality control was done by SEM photomicrograph and thermal shock test. The deposited target was irradiated at 30 microA current and 15 MeV proton beam for 12 min.