Compositional effects on the radiation response of Ge-doped silica-core optical fiber waveguides

The effect of variations in the Ge, B, P, and OH content on the radiation response of Ge-doped silica-core optical fiber waveguides has been measured at 0.82 and 1.3 microm. It has been established that variations in neither OH content nor Ge concentration affect the response of these fibers. B dopi...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Applied Optics 1980-09, Vol.19 (17), p.2910-2916
Hauptverfasser: Friebele, E J, Schultz, P C, Gingerich, M E
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The effect of variations in the Ge, B, P, and OH content on the radiation response of Ge-doped silica-core optical fiber waveguides has been measured at 0.82 and 1.3 microm. It has been established that variations in neither OH content nor Ge concentration affect the response of these fibers. B doping increases the loss at short times following pulsed irradiation, whereas P suppresses the intense Ge-related transient absorption at both 0.82 and 1.3 microm while inhibiting long-term recovery. Since there is a minimum in the induced loss near 1.1-1.2 microm in P-doped fibers, the damage at 1.55 microm is significantly higher than that at 1.3 microm.
ISSN:1559-128X
0003-6935
1539-4522
DOI:10.1364/AO.19.002910