Towards efficient and broadband four-wave-mixing using short-length dispersion tailored lead silicate holey fibers
We demonstrate four-wave-mixing based wavelength conversion at 1.55 mum in a 2.2 m-long dispersion-shifted lead-silicate holey fiber. For a pump peak power of ~6 W, a conversion efficiency of -6 dB is achieved over a 3-dB bandwidth of ~30 nm. Numerical simulations are used to predict the performance...
Gespeichert in:
Veröffentlicht in: | Optics express 2007-01, Vol.15 (2), p.596-601 |
---|---|
Hauptverfasser: | , , , , , , , , |
Format: | Artikel |
Sprache: | eng |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | We demonstrate four-wave-mixing based wavelength conversion at 1.55 mum in a 2.2 m-long dispersion-shifted lead-silicate holey fiber. For a pump peak power of ~6 W, a conversion efficiency of -6 dB is achieved over a 3-dB bandwidth of ~30 nm. Numerical simulations are used to predict the performance of the fiber for different experimental conditions and to address the potential of dispersion-tailored lead silicate holey fibers in wavelength conversion applications utilizing four-wave-mixing. It is shown that highly efficient and broadband wavelength conversion, covering the entire C-band, can be achieved for such fibers at reasonable optical pump powers and for fiber lengths as short as ~2 m. |
---|---|
ISSN: | 1094-4087 1094-4087 |
DOI: | 10.1364/oe.15.000596 |