In vitro wear assessment of titanium alloy teeth
Wear of commercially pure (CP) titanium prosthetic teeth has frequently been observed. The greatest wear has been found when the same grades of CP titanium are used for both maxillary and mandibular teeth. This study examined the wear behavior of teeth made with cast titanium alloy and compared thes...
Gespeichert in:
Veröffentlicht in: | Journal of prosthodontics 2002-12, Vol.11 (4), p.263-269, Article ajpro0110263 |
---|---|
Hauptverfasser: | , , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | Wear of commercially pure (CP) titanium prosthetic teeth has frequently been observed. The greatest wear has been found when the same grades of CP titanium are used for both maxillary and mandibular teeth. This study examined the wear behavior of teeth made with cast titanium alloy and compared these results with those for CP titanium and gold alloy teeth.
All tooth specimens were cast with grade 3 alpha titanium, 3 metastable beta alloys [Ti-15Mo-2.8Nb-0.2Si (Timetal 21 SRx), Ti-13Nb-13Zr, and Ti-15V-3Cr-3Sn-3Al], and 2 alpha+beta alloys (Ti-6Al-7Nb and Ti-6Al-4V). As a control, Type IV gold alloy was also cast conventionally. All teeth (both maxillary and mandibular) were secured in an in vitro 2-body wear testing apparatus that simulated chewing function (60 strokes/min; grinding distance, 2 mm under flowing water). Wear resistance was assessed as volume loss (mm(3)) at 5 kgf (grinding force) after 50,000 strokes. The results (n = 5) were analyzed using analysis of variance or Fisher's exact test (alpha = 0.05).
Of the titanium teeth, the wear of 2 of the metastable beta alloys (Timetal 21 SRx and Ti-15V-3Cr-3Sn-3Al) was found to be significantly (p |
---|---|