Sealing and dentin bond strengths of adhesive systems
The objectives of this research were (1) to analyze the variations of the permeability of dentin after restoration with two polyacid-modified resin composites (Compoglass, Dyract) and four single-bottle adhesives (Prime & Bond 2.0, Syntac Single Component, OptiBond Solo, and Single Bond--Scotch...
Gespeichert in:
Veröffentlicht in: | Operative dentistry 1999-07, Vol.24 (4), p.194-202 |
---|---|
Hauptverfasser: | , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The objectives of this research were (1) to analyze the variations of the permeability of dentin after restoration with two polyacid-modified resin composites (Compoglass, Dyract) and four single-bottle adhesives (Prime & Bond 2.0, Syntac Single Component, OptiBond Solo, and Single Bond--Scotch Bond 1 in Europe--immediately (approximately 1 hour) after insertion. A perfusion system with distilled water was used at a pressure of 32.5 cm of water; (2) to study the bond strength of their interfaces; and (3) to find the correlation, if any, between both parameters. None of the materials used produced a complete cessation in fluid filtration. Tensile bond strengths were very low (maximum: P&B = 3.96 MPa) probably because of the very large bonding surfaces used (mean bonded surface area = 88.8 mm2). No significant correlation was found between tensile bond strength and the sealing ability for any material. |
---|---|
ISSN: | 0361-7734 |