Autoclaved brick from low-silicon tailings

The load-bearing brick is made from low-silicon tailings by pressing and autoclaving process, in the presence of alkali-activated slag/fly ash cementing material (AAFSC). Tailings accounts for 83% of the total mass of the brick. The compressive strength of the brick is up to 16.1 MPa, bending streng...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Construction & building materials 2009, Vol.23 (1), p.538-541
Hauptverfasser: Zhao, Feng-qing, Zhao, Jing, Liu, Hong-jie
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The load-bearing brick is made from low-silicon tailings by pressing and autoclaving process, in the presence of alkali-activated slag/fly ash cementing material (AAFSC). Tailings accounts for 83% of the total mass of the brick. The compressive strength of the brick is up to 16.1 MPa, bending strength 3.8 MPa, and with low drying shrinkage and good freeze–thaw resistance. Some factors influencing the mechanical strength of the brick including forming pressure, forming water content and curing regime, are investigated. The hydration products, freeze–thaw durability and anti-carbonation characteristics of the products are discussed.