Phosphorus induced hydrothermal stability and enhanced catalytic activity of ZSM-5 in methanol to DME conversion

The change in properties of ZSM-5 samples was achieved by treatment with phosphorus compounds (trimethyl phosphite or phosphoric acid) and the resultant materials were characterized by N 2 adsorption, NH 3-TPD, 27Al, and 31P MAS NMR techniques. The phosphorus-treated HZSM-5 (P/ZSM-5) samples exhibit...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Fuel (Guildford) 2009-10, Vol.88 (10), p.1915-1921
Hauptverfasser: Lee, Yun-Jo, Kim, Jung Mi, Bae, Jong Wook, Shin, Chae-Ho, Jun, Ki-Won
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The change in properties of ZSM-5 samples was achieved by treatment with phosphorus compounds (trimethyl phosphite or phosphoric acid) and the resultant materials were characterized by N 2 adsorption, NH 3-TPD, 27Al, and 31P MAS NMR techniques. The phosphorus-treated HZSM-5 (P/ZSM-5) samples exhibited lower acidity, higher hydrothermal stability and improved dimethyl ether (DME) selectivity in methanol conversion when compared to the phosphorus-free HZSM-5. 27Al, and 31P MAS NMR results revealed that the added P indeed interacted with the ZSM-5 framework and is responsible for the changes observed in the catalytic properties. The interaction caused the decrease in strong acid sites on one hand and creation of new acid sites (NH 3-TPD) on the other, in P/ZSM-5 samples. The studies indicated the need of optimizing the P loading, where the positive role of P on the catalytic activity was observed to be maximum at P/Al molar ratio of 1.05.
ISSN:0016-2361
1873-7153
DOI:10.1016/j.fuel.2009.04.007