Annealing effects of Ga@d2O@d3-ZnO core-shell heteronanowires
We prepared ZnO-coated Ga@d2O@d3 nanowires and investigated changes in the morphological, structural, and photoluminescence (PL) characteristics resulting from application of a thermal annealing process. With the thermal annealing at 800@uoC, defect-associated PL peaks (2.2 and 2.6eV) have been inte...
Gespeichert in:
Veröffentlicht in: | Materials science & engineering. B, Solid-state materials for advanced technology Solid-state materials for advanced technology, 2009-06, Vol.163 (1), p.44-47 |
---|---|
Hauptverfasser: | , , , , |
Format: | Artikel |
Sprache: | eng |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | 47 |
---|---|
container_issue | 1 |
container_start_page | 44 |
container_title | Materials science & engineering. B, Solid-state materials for advanced technology |
container_volume | 163 |
creator | Kim, H W Lee, J W Kebede, M A Kim, H S Lee, C |
description | We prepared ZnO-coated Ga@d2O@d3 nanowires and investigated changes in the morphological, structural, and photoluminescence (PL) characteristics resulting from application of a thermal annealing process. With the thermal annealing at 800@uoC, defect-associated PL peaks (2.2 and 2.6eV) have been intensified with respect to the UV peak, and a new 2.8eV-peak has been generated. Possible emission mechanisms are also discussed. |
doi_str_mv | 10.1016/j.mseb.2009.04.018 |
format | Article |
fullrecord | <record><control><sourceid>proquest</sourceid><recordid>TN_cdi_proquest_miscellaneous_34497700</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>34497700</sourcerecordid><originalsourceid>FETCH-proquest_miscellaneous_344977003</originalsourceid><addsrcrecordid>eNqNy7sOgjAUgOEOmoiXF3Dq5NZ6WlBkMMEYLxuLkwupcBAItMrB-Po6-ABO__L9jM0VSAVqvaxlS3iTGiCSEEhQmwHzINJKrBSEIzYmqgFAaa09tt1Zi6ap7J1jUWDWE3cFP5k410mc--JqE565DgWV2DS8xB47Z41176pDmrJhYRrC2a8TtjgeLvuzeHTu-ULq07ai7Dsai-5FqR8EURgC-H_DD_JXP_Y</addsrcrecordid><sourcetype>Aggregation Database</sourcetype><iscdi>true</iscdi><recordtype>article</recordtype><pqid>34497700</pqid></control><display><type>article</type><title>Annealing effects of Ga@d2O@d3-ZnO core-shell heteronanowires</title><source>Access via ScienceDirect (Elsevier)</source><creator>Kim, H W ; Lee, J W ; Kebede, M A ; Kim, H S ; Lee, C</creator><creatorcontrib>Kim, H W ; Lee, J W ; Kebede, M A ; Kim, H S ; Lee, C</creatorcontrib><description>We prepared ZnO-coated Ga@d2O@d3 nanowires and investigated changes in the morphological, structural, and photoluminescence (PL) characteristics resulting from application of a thermal annealing process. With the thermal annealing at 800@uoC, defect-associated PL peaks (2.2 and 2.6eV) have been intensified with respect to the UV peak, and a new 2.8eV-peak has been generated. Possible emission mechanisms are also discussed.</description><identifier>ISSN: 0921-5107</identifier><identifier>DOI: 10.1016/j.mseb.2009.04.018</identifier><language>eng</language><ispartof>Materials science & engineering. B, Solid-state materials for advanced technology, 2009-06, Vol.163 (1), p.44-47</ispartof><lds50>peer_reviewed</lds50><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><link.rule.ids>314,780,784,27924,27925</link.rule.ids></links><search><creatorcontrib>Kim, H W</creatorcontrib><creatorcontrib>Lee, J W</creatorcontrib><creatorcontrib>Kebede, M A</creatorcontrib><creatorcontrib>Kim, H S</creatorcontrib><creatorcontrib>Lee, C</creatorcontrib><title>Annealing effects of Ga@d2O@d3-ZnO core-shell heteronanowires</title><title>Materials science & engineering. B, Solid-state materials for advanced technology</title><description>We prepared ZnO-coated Ga@d2O@d3 nanowires and investigated changes in the morphological, structural, and photoluminescence (PL) characteristics resulting from application of a thermal annealing process. With the thermal annealing at 800@uoC, defect-associated PL peaks (2.2 and 2.6eV) have been intensified with respect to the UV peak, and a new 2.8eV-peak has been generated. Possible emission mechanisms are also discussed.</description><issn>0921-5107</issn><fulltext>true</fulltext><rsrctype>article</rsrctype><creationdate>2009</creationdate><recordtype>article</recordtype><recordid>eNqNy7sOgjAUgOEOmoiXF3Dq5NZ6WlBkMMEYLxuLkwupcBAItMrB-Po6-ABO__L9jM0VSAVqvaxlS3iTGiCSEEhQmwHzINJKrBSEIzYmqgFAaa09tt1Zi6ap7J1jUWDWE3cFP5k410mc--JqE565DgWV2DS8xB47Z41176pDmrJhYRrC2a8TtjgeLvuzeHTu-ULq07ai7Dsai-5FqR8EURgC-H_DD_JXP_Y</recordid><startdate>20090625</startdate><enddate>20090625</enddate><creator>Kim, H W</creator><creator>Lee, J W</creator><creator>Kebede, M A</creator><creator>Kim, H S</creator><creator>Lee, C</creator><scope>7SR</scope><scope>8BQ</scope><scope>8FD</scope><scope>JG9</scope></search><sort><creationdate>20090625</creationdate><title>Annealing effects of Ga@d2O@d3-ZnO core-shell heteronanowires</title><author>Kim, H W ; Lee, J W ; Kebede, M A ; Kim, H S ; Lee, C</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-proquest_miscellaneous_344977003</frbrgroupid><rsrctype>articles</rsrctype><prefilter>articles</prefilter><language>eng</language><creationdate>2009</creationdate><toplevel>peer_reviewed</toplevel><toplevel>online_resources</toplevel><creatorcontrib>Kim, H W</creatorcontrib><creatorcontrib>Lee, J W</creatorcontrib><creatorcontrib>Kebede, M A</creatorcontrib><creatorcontrib>Kim, H S</creatorcontrib><creatorcontrib>Lee, C</creatorcontrib><collection>Engineered Materials Abstracts</collection><collection>METADEX</collection><collection>Technology Research Database</collection><collection>Materials Research Database</collection><jtitle>Materials science & engineering. B, Solid-state materials for advanced technology</jtitle></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext</fulltext></delivery><addata><au>Kim, H W</au><au>Lee, J W</au><au>Kebede, M A</au><au>Kim, H S</au><au>Lee, C</au><format>journal</format><genre>article</genre><ristype>JOUR</ristype><atitle>Annealing effects of Ga@d2O@d3-ZnO core-shell heteronanowires</atitle><jtitle>Materials science & engineering. B, Solid-state materials for advanced technology</jtitle><date>2009-06-25</date><risdate>2009</risdate><volume>163</volume><issue>1</issue><spage>44</spage><epage>47</epage><pages>44-47</pages><issn>0921-5107</issn><abstract>We prepared ZnO-coated Ga@d2O@d3 nanowires and investigated changes in the morphological, structural, and photoluminescence (PL) characteristics resulting from application of a thermal annealing process. With the thermal annealing at 800@uoC, defect-associated PL peaks (2.2 and 2.6eV) have been intensified with respect to the UV peak, and a new 2.8eV-peak has been generated. Possible emission mechanisms are also discussed.</abstract><doi>10.1016/j.mseb.2009.04.018</doi></addata></record> |
fulltext | fulltext |
identifier | ISSN: 0921-5107 |
ispartof | Materials science & engineering. B, Solid-state materials for advanced technology, 2009-06, Vol.163 (1), p.44-47 |
issn | 0921-5107 |
language | eng |
recordid | cdi_proquest_miscellaneous_34497700 |
source | Access via ScienceDirect (Elsevier) |
title | Annealing effects of Ga@d2O@d3-ZnO core-shell heteronanowires |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-20T00%3A10%3A42IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-proquest&rft_val_fmt=info:ofi/fmt:kev:mtx:journal&rft.genre=article&rft.atitle=Annealing%20effects%20of%20Ga@d2O@d3-ZnO%20core-shell%20heteronanowires&rft.jtitle=Materials%20science%20&%20engineering.%20B,%20Solid-state%20materials%20for%20advanced%20technology&rft.au=Kim,%20H%20W&rft.date=2009-06-25&rft.volume=163&rft.issue=1&rft.spage=44&rft.epage=47&rft.pages=44-47&rft.issn=0921-5107&rft_id=info:doi/10.1016/j.mseb.2009.04.018&rft_dat=%3Cproquest%3E34497700%3C/proquest%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_pqid=34497700&rft_id=info:pmid/&rfr_iscdi=true |