Improved Oxidation Resistance of Zirconium Diboride by Tungsten Carbide Additions

The effect of tungsten carbide (WC) additions on the oxidation resistance of zirconium diboride (ZrB2) was studied. Zirconium diboride ceramics, nominally pure and with the addition of 4 mol% WC, were densified by pressureless sintering. During densification, the WC that was added to the ceramic dis...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of the American Ceramic Society 2008-11, Vol.91 (11), p.3530-3535
Hauptverfasser: Zhang, Shi C., Hilmas, Greg E., Fahrenholtz, William G.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The effect of tungsten carbide (WC) additions on the oxidation resistance of zirconium diboride (ZrB2) was studied. Zirconium diboride ceramics, nominally pure and with the addition of 4 mol% WC, were densified by pressureless sintering. During densification, the WC that was added to the ceramic dissolved into the ZrB2 matrix, forming a solid solution. Oxidation behavior was evaluated using thermal gravimetric analysis up to 1500°C and isothermal furnace oxidation at 1500° and 1600°C. The WC additions reduced both the weight gain and the oxide scale thickness. After oxidation at 1600°C for 3 h, the mass gain decreased from 22 mg/cm2 for nominally pure ZrB2 to 8 mg/cm2 for the WC‐containing ceramic. Analysis showed that the WC additions improved the oxidation resistance of ZrB2 by promoting densification of the zirconia scale formed during oxidation through liquid‐phase sintering.
ISSN:0002-7820
1551-2916
DOI:10.1111/j.1551-2916.2008.02713.x