Fabrication of fluorocarbon terminated DLC thin film using soft X-ray

The control of wettability on a diamond-like carbon (DLC) thin film was carried out by exposing the film to synchrotron radiation (SR) ranging 50–1000 e V under perfluorohexane (C 6F 14) gas atmosphere. The contact angle of the DLC surface with a water droplet was found to increase from 73° to 114°...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Diamond and related materials 2008-04, Vol.17 (4), p.655-658
Hauptverfasser: Yamada, N., Kanda, K., Saikubo, A., Niibe, M., Haruyama, Y., Matsui, S.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The control of wettability on a diamond-like carbon (DLC) thin film was carried out by exposing the film to synchrotron radiation (SR) ranging 50–1000 e V under perfluorohexane (C 6F 14) gas atmosphere. The contact angle of the DLC surface with a water droplet was found to increase from 73° to 114° by the SR irradiation under C 6F 14 gas atmosphere. The chemical components variations of the DLC surface were studied using X-ray photoelectron spectroscopy and the modified DLC film with F was studied using near-edge X-ray absorption fine structure spectroscopy. By mounting the new sample holder for the parallel SR irradiation, we succeeded in preventing secondary reaction of deposited material and controlling the contact angle of the fluorocarbon modified DLC surface.
ISSN:0925-9635