Effect of heat treatment on the performance of TiO2-Pt/CNT catalysts for methanol electro-oxidation

TiO2-Pt/CNT catalysts before and after heat treatment were prepared. Their catalytic activities for methanol and CO electro-oxidation were studied in detail. The results showed that the proper amount of hydrous TiO2 in TiO2-Pt/CNTs (e.g. heated at 200 deg C for 2h) was favorable for enhancing the ca...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Electrochimica acta 2008-04, Vol.53 (10), p.3708-3713
Hauptverfasser: Song, Huanqiao, Qiu, Xinping, Li, Fushen
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:TiO2-Pt/CNT catalysts before and after heat treatment were prepared. Their catalytic activities for methanol and CO electro-oxidation were studied in detail. The results showed that the proper amount of hydrous TiO2 in TiO2-Pt/CNTs (e.g. heated at 200 deg C for 2h) was favorable for enhancing the catalytic activity of Pt/CNTs, which provided evidence for bi-functional mechanism. The studies on the catalysts with different TiO2/Pt molar ratio displayed that the optimum molar ratio varied with the increase of heat treatment temperature. It was found that the optimum molar ratio of TiO2/Pt was at 1:2 for the catalysts without heat treatment and was at 1:1 for the catalysts by heat treatment at 500 deg C. This fact was ascribed to the difference in compact degree between TiO2 and Pt/CNTs before and after heat treatment. Considering the influence of heating temperature, it was found that TiO2-Pt/CNT catalyst heated at 200 deg C for 2h had better catalytic activity for methanol oxidation.
ISSN:0013-4686
1873-3859
DOI:10.1016/j.electacta.2007.11.080