Suppressing Oxygen Adsorption on Bulk Arsenic and 2D Arsenic Nanoflake Surfaces: The Role of Sb Doping
The susceptibility of bulk and exfoliated nanolayered arsenic to oxidation has been a significant obstacle limiting their widespread application and safe disposal. Here we report a controllable antimony-doped (Sb-doped) method via chemical vapor transport (CVT) with SnI4 as a transport agent to prep...
Gespeichert in:
Veröffentlicht in: | ACS applied materials & interfaces 2024-12, Vol.16 (48), p.66673-66685 |
---|---|
Hauptverfasser: | , , , , , , , , , , , |
Format: | Artikel |
Sprache: | eng |
Schlagworte: | |
Online-Zugang: | Volltext |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The susceptibility of bulk and exfoliated nanolayered arsenic to oxidation has been a significant obstacle limiting their widespread application and safe disposal. Here we report a controllable antimony-doped (Sb-doped) method via chemical vapor transport (CVT) with SnI4 as a transport agent to prepare the bulk arsenic. After 96 h of exposure to air, the oxygen content on the surface of Sb-doped arsenic with SnI4 is 67% lower compared to the undoped arsenic with SnI4, and 89% lower than the control group (undoped arsenic without SnI4). Notably, Sb-doped arsenic is found to be easier and better exfoliated into two-dimensional (2D) nanoflakes with an average diameter of approximately 180 nm and a thickness of 4–5 nm. Sb doping reduces the surface oxygen content of exfoliated arsenic nanoflakes by 48% after 48 h of oxidation. Comprehensive experimental investigations combined with first-principles calculations demonstrate that the antioxidation improvements resulting from Sb-doping are due to the decreased adsorption energies of I2 on the (012) and (003) surfaces of Sb-doped arsenic, while the adsorption energies of O2 increased compared to the corresponding surfaces of undoped arsenic. The enhanced long-term stability in both bulk and layered Sb-doped arsenic presents a promising avenue for further advanced applications. |
---|---|