Production of pyrolytic lignin for the phenolic resin synthesis via fast pyrolysis

Recycling of waste wood into resol type phenol-formaldehyde (PF) resins via fast pyrolysis was demonstrated. Waste wood collected from the building demolition site in Finland was pyrolyzed with 20 kg/h circulating fluidized bed pyrolysis pilot unit. Pilot was operated with high organic liquid yield...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of analytical and applied pyrolysis 2023-11, Vol.176, p.106239, Article 106239
Hauptverfasser: Pienihäkkinen, Elmeri, Stamatopoulos, Ioannis, Krassa, Poppy, Svensson, Ingemar, Ohra-aho, Taina, Lindfors, Christian, Oasmaa, Anja
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Recycling of waste wood into resol type phenol-formaldehyde (PF) resins via fast pyrolysis was demonstrated. Waste wood collected from the building demolition site in Finland was pyrolyzed with 20 kg/h circulating fluidized bed pyrolysis pilot unit. Pilot was operated with high organic liquid yield (60 wt% on average) and the produced fast pyrolysis bio-oil was fractionated by water addition into aqueous phase and water insoluble phase. The obtained fractions were characterized, and the water-insoluble viscous lignin fraction was used in the synthesis of PF-resins. Commercial phenol was successfully replaced by pyrolytic lignin fraction at 10 wt%, 20 wt%, 30 wt%, 40 wt% and 50 wt% producing resins of low in free formaldehyde content, but resins with high replacement ratio exhibited higher viscosities. The use of H₂O/n-butanol mixture as solvent at a ratio 70:30 wt/wt% proved capable to prolong the storage time of the resin and helped to maintain the viscosity at acceptable values for at least 2 weeks before their use in the targeted application. Finally, the gluing performance of the resins was evaluated by measuring the tensile shear strength of lap joints formed by gluing 5 mm thick beech wood veneers. All the produced resins fulfilled a dry strength limit of ≥ 10 N/mm². Wet strength limit ≥ 7 N/mm² was fulfilled by the resins with the replacement ratio up 40 wt%, but resins with replacement ratio of 50 wt% had somewhat reduced wet strength. These results confirm a promising protentional application of pyrolysis derived lignin fraction in phenolic wood adhesives, at least in dry conditions.