Hydrothermal synthesis of nickel ferrite powders, their properties and sintering

NiFe 2O 4 powders were synthesized by co-precipitation with ammonia solution using aqueous solution of NiCl 2 and FeCl 3 followed by hydrothermal treatment of the precipitate. It was found that crystallization in water led to nanometric in size and isometric in shape crystallites, whereas crystalliz...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of the European Ceramic Society 2007, Vol.27 (2), p.723-727
Hauptverfasser: Bućko, Mirosław M., Haberko, Krzysztof
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:NiFe 2O 4 powders were synthesized by co-precipitation with ammonia solution using aqueous solution of NiCl 2 and FeCl 3 followed by hydrothermal treatment of the precipitate. It was found that crystallization in water led to nanometric in size and isometric in shape crystallites, whereas crystallization in sodium hydroxide solution results in particles of well defined walls. Generally, particles crystallized in water were smaller and their particle size distribution was narrower than those crystallized in NaOH solution. Behaviour of the powders under dry compaction and sintering strongly depended on the powder morphology. The powder crystallized in NaOH solution gave compacts of higher density and sintered density of this powder was also higher than that of the powder processed in water.
ISSN:0955-2219
1873-619X
DOI:10.1016/j.jeurceramsoc.2006.04.052