Arsenite retention properties of water-soluble metal-polymers

The properties of water-soluble metal-polymers to retain As(III) from aqueous solution are investigated. Poly(acrylic acid)s with different tin contents are prepared. Amounts of 3, 5, 10, and 20 wt % of tin are added to the polymer. The metal compositions are evaluated by thermogravimetry (TG-DSC) a...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of applied polymer science 2007-11, Vol.106 (3), p.1889-1894
Hauptverfasser: Rivas, Bernabé L, Aguirre, María del Carmen
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The properties of water-soluble metal-polymers to retain As(III) from aqueous solution are investigated. Poly(acrylic acid)s with different tin contents are prepared. Amounts of 3, 5, 10, and 20 wt % of tin are added to the polymer. The metal compositions are evaluated by thermogravimetry (TG-DSC) and atomic absorption spectroscopy. Structural properties are analyzed by infrared and ¹H nuclear magnetic resonance spectroscopy, and X-ray diffraction. Additionally, specific surface area was measured using CO₂ as adsorbate. Arsenic retention properties are studied using the liquid-phase polymer-based retention (LPR) technique. The polymers can bind arsenic species from an aqueous solution in the pH range 4-8. The studies show that the retention capacity is a function of tin content and polymer concentration. At pH 8, the following mol ratios poly(AA)-Sn : As(III) are analyzed: 600 : 1, 400 : 1, 200 : 1, 100 : 1, and 20 : 1. The highest retention, 80%, is obtained with poly(AA)-Sn at 10 and 20 wt % of tin at mole ratios 400 : 1, and at nearly to 20 : 1 or 40 : 1 Sn-As(III). The highest retention is observed at pH 8 and 4. © 2007 Wiley Periodicals, Inc. J Appl Polym Sci 2007
ISSN:0021-8995
1097-4628
DOI:10.1002/app.26737