High coercivity in Sm5Fe17 melt-spun ribbon

Sm-Fe binary alloy with the hard magnetic Sm5Fe17 phase was produced by melt-spinning followed by heat treatment. The magnetic properties of the Sm-Fe melt-spun ribbon depended on the annealing temperature. The highest coercivity, iHc=1.90MAm-1, was obtained by annealing the Sm-Fe melt-spun ribbon f...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of alloys and compounds 2007-08, Vol.440 (1-2), p.315-318
1. Verfasser: SAITO, Tetsuji
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:Sm-Fe binary alloy with the hard magnetic Sm5Fe17 phase was produced by melt-spinning followed by heat treatment. The magnetic properties of the Sm-Fe melt-spun ribbon depended on the annealing temperature. The highest coercivity, iHc=1.90MAm-1, was obtained by annealing the Sm-Fe melt-spun ribbon for 1h at 923K. The coercivity of the Sm5Fe17 melt-spun ribbon was attributed to the grain size of the hard magnetic Sm5Fe17 phase.
ISSN:0925-8388
1873-4669
DOI:10.1016/j.jallcom.2006.09.011