Temperature dependence of misfit strains of δ-hydrides of zirconium

The misfit strains of both the isotopic forms of zirconium hydrides, viz., δ-ZrH x and δ-ZrD x , precipitated in zirconium were computed in the temperature range of 298–773 K and for 1.5 ≤ x ≤ 1.7, using the methodology proposed by Carpenter. Misfit strains along (0 0 0 1) plane and normal to it wer...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Journal of alloys and compounds 2007-06, Vol.436 (1), p.150-154
Hauptverfasser: Singh, R.N., Ståhle, P., Massih, A.R., Shmakov, A.A.
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The misfit strains of both the isotopic forms of zirconium hydrides, viz., δ-ZrH x and δ-ZrD x , precipitated in zirconium were computed in the temperature range of 298–773 K and for 1.5 ≤ x ≤ 1.7, using the methodology proposed by Carpenter. Misfit strains along (0 0 0 1) plane and normal to it were observed to increase with increase in temperature for both the isotopic forms of hydrides. For a given isotopic atomic fraction, the misfit strains for deuteride were smaller than the corresponding values for hydride and with increase in atomic fraction of hydrogen isotopes, the misfit strains increased.
ISSN:0925-8388
1873-4669