Low Temperature Sintering (Ba1-xSrx)TiO3 Ceramics by Using CuO-TiO2 Mixture as Sintering Aid

1wt% CuO-TiO2 (molar ratio, CuO/TiO2= 1) mixture is added as the liquid phase sintering aid to develop the sintering and dielectric characteristics of (Ba1-xSrx)TiO3 (x=0, 0.1, and 0.2) ceramics. The crystal characteristics of calcined (Ba1-xSrx)TiO3 powders and sintered (Ba1-xSrx)TiO3 ceramics are...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Key engineering materials 2007-01, Vol.336-338, p.62-65
Hauptverfasser: Diao, Chien Chen, Chan, Chao Chin, Yang, Cheng Fu, Su, Chean Cheng
Format: Artikel
Sprache:eng
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:1wt% CuO-TiO2 (molar ratio, CuO/TiO2= 1) mixture is added as the liquid phase sintering aid to develop the sintering and dielectric characteristics of (Ba1-xSrx)TiO3 (x=0, 0.1, and 0.2) ceramics. The crystal characteristics of calcined (Ba1-xSrx)TiO3 powders and sintered (Ba1-xSrx)TiO3 ceramics are developed by using X-ray diffraction method. The calcined (Ba1-xSrx)TiO3 powders and 1050oC-sintered (Ba1-xSrx)TiO3 ceramics reveal a tetragonal or pseudo-cubic structure and the 1150oC-sintered(Ba1-xSrx)TiO3 ceramics reveal a tetragonal structure. Sintered at 1100oC, the (Ba1-xSrx)TiO3 ceramics present a porous structure; Sintered at 1150oC, the (Ba1-xSrx)TiO3 ceramics present a uniform growth. The grain size decreases with the increase of SrO content. In this study, the dielectric characteristics of CuO-TiO2 mixture-fluxed (Ba1-xSrx)TiO3 ceramics are also developed.
ISSN:1013-9826
1662-9795
1662-9795
DOI:10.4028/www.scientific.net/KEM.336-338.62