Anelastic relaxation in SrTiO3 with O vacancies and H

We present the results of anelastic relaxation experiments (2-30 kHz) on ceramic SrTiO3 subjected to reduction in H2 atmosphere, which yields a balance between oxygen vacancy (VO) and (OH)(-) defects. The resulting anelastic spectrum contains, besides the well known structural transformation near 11...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Veröffentlicht in:Materials science & engineering. A, Structural materials : properties, microstructure and processing Structural materials : properties, microstructure and processing, 2006-12, Vol.442 (1-2), p.55-58
Hauptverfasser: CORDERO, F, FRANCE, A, CALDERONE, V. R, NANNI, P, BUSCAGLIA, V
Format: Artikel
Sprache:eng
Schlagworte:
Online-Zugang:Volltext
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:We present the results of anelastic relaxation experiments (2-30 kHz) on ceramic SrTiO3 subjected to reduction in H2 atmosphere, which yields a balance between oxygen vacancy (VO) and (OH)(-) defects. The resulting anelastic spectrum contains, besides the well known structural transformation near 110K, several thermally activated relaxation processes between 200 and 700 K. The two main elastic energy loss peaks are proposed to provide the first measurement of the hopping rate of Vo and (OH)(-) defects in pure SrTiO3.
ISSN:0921-5093
1873-4936